SEBS基柔性相变材料的制备及其性能研究
Preparation and performance investigation of SEBS-based flexible phase change materials
投稿时间:2024-09-03  
DOI:10.13259/j.cnki.eri.2026.03.007
中文关键词:  苯乙烯–乙烯–丁二烯–苯乙烯嵌段共聚物  膨胀石墨  相变材料  柔性  性能分析
英文关键词:styrene-ethylene-butylene-styrene block copolymer  expanded graphite  phase change materials  flexibility  property analysis
基金项目:
作者单位
陆馨仪 同济大学 汽车与能源学院,上海 201804 
吴俐俊 同济大学 汽车与能源学院,上海 201804 
摘要点击次数: 0
全文下载次数: 0
中文摘要:
      为解决储能设备热管理系统中固–液相变材料易断裂、泄漏和导热系数低的问题,以石蜡(PA)为相变基体材料,苯乙烯–乙烯–丁二烯–苯乙烯嵌段共聚物(SEBS)为形状稳定剂,膨胀石墨(EG)为导热增强剂,采用熔融共混法制备了6种不同配比的柔性复合相变材料,并通过差示扫描量热法、泄漏实验、扫描电镜、热常数分析和热失重分析等手段表征样品的结构、相变性能和热性能。结果表明:当PA和SEBS质量比为4∶1、EG添加量(质量分数)为5%时复合相变材料的综合性能最优,相变温度为39.9 ℃,相变潜热为191.0 J/g;60 ℃下泄漏率仅为0.71%,形状稳定性最佳;导热系数达0.788 W/(m·K),为纯PA的3.8倍。本研究为柔性复合相变材料的研发及其在储能设备热管理中的应用提供了实验依据。
英文摘要:
      To address the problems of easy fracture, leakage, and low thermal conductivity of solid-liquid phase change materials in thermal management systems for energy storage devices, six flexible composite phase change materials with different ratios were prepared by melt blending, using paraffin (PA) as the phase change matrix, styrene-ethylene-butylene-styrene block copolymer (SEBS) as the shape stabilizer, and expanded graphite (EG) as the thermal conductivity enhancer. The structure, phase transition properties, and thermal properties of the samples were characterized by differential scanning calorimetry (DSC), leakage tests, scanning electron microscopy (SEM), thermal constant analysis, and thermogravimetric analysis (TGA). The results showed that the composite with a PA-to-SEBS mass ratio of 4∶1 and 5% EG addition exhibited a phase change temperature of 39.9 ℃ and a latent heat of 191.0 J/g, a leakage rate of 0.71% (the best shape stability among all formulations), and a thermal conductivity of 0.788 W/(m·K), which was approximately 3.8 times that of pure PA. This study provides an experimental basis for the development of flexible composite phase change materials and their application in thermal management of energy storage devices.